Muscle Cars & Hot Rods Episode 7


Jeff does some lead repair on the 34 Ford street rod.

Related Posts

Tags : , , ,

Google Reader Yahoo Facebook Twitter Digg FriendFeed Delicious Google Translate
This entry was posted onNovember 22nd, 2009 at 7:45 am. You can follow any responses to this entry through the RSS 2.0. Responses are currently closed, but you can Trackback..

4 Responses

Comments(4)Trackbacks(0)

  1. fxrjohnny

    So you heat the panel, and push the lead to it or heat the lead too? It seems like it does not take too much heat to melt the lead. I have not tried this yet, but want as much imfo as i can get first. Thanks for the vid, shows step by step and the process involved. Later.

    November 22, 2009 7:57 am | #1
  2. jamesfreddys

    you tin the metal first then you heat the metal and the lead, it’s very similar to soildering in fact some call it body soildering.

    November 22, 2009 8:08 am | #2
  3. MeyeMaybach

    like the stang

    November 22, 2009 8:22 am | #3
  4. tbr340

    Sweet. Very nice work. Thanks for vid. keep up the good work.